Boron B (Borium) an alloying element in steel and nickel alloys

Boron B (Borium) – an alloying element in steel and nickel alloys. It influences hardenability, microstructure, and material properties.

Boron (B) is a semimetal that, even in very small amounts, can significantly alter the behavior of steel during heat treatment. Boron's most well-known use is to increase the hardenability of structural steels , meaning their ability to form a martensitic structure in larger cross-sections or with less intense cooling. Unlike many traditional alloying additives, such as chromium (Cr) , manganese (Mn) , or molybdenum (Mo) , boron is typically used for this purpose in quantities measured in parts per million (ppm).

Boron's importance, however, is not limited to hardening steels. This element influences grain boundaries, the formation of nitrides and borides, the behavior of materials at high temperatures, and fracture toughness. In some nickel superalloys, carefully controlled amounts of boron can increase durability under prolonged thermal stress. Meanwhile, the diffusion boronizing process uses boron to produce very hard surface layers. These are three distinct applications that require separate discussion.

Boron – basic information about the chemical element

Boron belongs to group 13 and period 2 of the periodic table. It is a semimetal whose properties differ from those of typical structural metals: it has a hard, brittle structure, strong chemical bonds, and a high tendency to form compounds with other elements. In nature, it occurs primarily in the form of borate minerals, not as a free element.

PropertyValue or characteristic
Name of the elementBoron
Chemical symbolB
Atomic number5
Relative atomic mass10,81
Group / period13 / 2
Electron configuration[He] 2s² 2p¹
State of matter at 20°CSolid
DensityAbout 2,34 g/cm³ (for crystalline boron, depending on variety)
Melting temperatureAbout 2077°C
Boiling pointAbout 4000°C
Natural stable isotopes¹⁰B and ¹¹B

The temperatures and densities quoted refer to elemental boron. They should not be confused with the melting point of steel containing trace boron or with the temperatures of thermochemical treatment processes.

The history of the discovery and industrial importance of boron

Boron compounds, particularly borax, were used long before the element itself was isolated, including as fluxes in metalworking. In 1808, boron was independently obtained by French researchers Joseph Louis Gay-Lussac and Louis Jacques Thénard, and British chemist Humphry Davy. However, the preparations obtained at that time were not chemically pure boron. Further purification methods were developed in the 19th and 20th centuries.

In metallurgy, the discovery that a small addition of boron can alter the course of structural changes during steel cooling proved particularly important. The development of precise trace element assays and smelting technologies subsequently allowed for the exploitation of this effect in structural, automotive, and specialty steels.

Why does such a small amount of boron affect steel?

The effect of boron is primarily related to its segregation to the austenite grain boundaries . During appropriate heating and cooling, some of the boron atoms dissolved in the matrix migrate to the grain boundaries. This can limit the formation of ferrite nuclei at these boundaries and delay the onset of austenite diffusion transformations.

As a result, at a given cooling rate, a larger proportion of austenite can survive into the martensitic transformation region. The steel becomes more hardenable, and the required post-hardening properties can be achieved at greater cross-sectional depths. However, the magnitude of the effect depends on the steel composition, the amount of boron remaining in solution, the thermal history, and the cooling parameters.

It is crucial to distinguish between total boron and effective boron. Chemical analysis may reveal a certain B content, but if a significant portion of it is bound in stable precipitates, it will not affect hardenability in the way expected for boron dissolved in austenite.

Boron and hardenability, hardness and strength of steel – differences

Material descriptions often use the simplified notion that boron "increases the hardness of steel." This isn't precise enough. Hardenability refers to the steel's ability to form a hardening structure under specific cooling conditions; hardness , on the other hand, is a property of the finished material, dependent primarily on its microstructure, carbon (C) content , and heat treatment.

  • Temper: trace amounts of appropriately active boron can significantly increase it.
  • Hardness after tempering: in a given area of ​​the product may be greater if more martensite is formed there thanks to boron; however, boron does not replace the role of carbon in shaping the hardness of martensite.
  • Tensile strength Rm: may increase after proper heat treatment, especially when the proportion of martensite in the cross-section increases.
  • Yield strength: depends on the obtained structure and state of processing; the designation "boron steel" alone does not determine its value.
  • Plasticity and impact strength: may decrease with increasing hardness or the formation of unfavorable precipitates, therefore it is necessary to select the heat treatment for the application.

For example, two steels with similar carbon content can achieve similar maximum hardness in a fully hardened thin sample, but a steel with a carefully selected boron addition can exhibit a significantly greater hardening depth in a large-section component. This effect justifies the economic use of boron.

How much boron is added to steel?

In many low- and medium-carbon boron steels intended for hardening, the boron content is approximately in the range of 0,0005–0,0050% by weight , or approximately 5–50 ppm . However, this is not a universal formula or a range applicable to all grades. The optimum range may be narrower for a specific material, and its location depends on factors such as the nitrogen, titanium, and molybdenum content, and the austenitizing temperature.

Boron, % by weightBoron, ppm by massMeaning
0,0005 %5 ppmA trace additive with possible metallurgical effects
0,0010 %10 ppmExample level in controlled hardenability steels
0,0030 %30 ppmTypical order of magnitude of addition in some boron steels
0,0050 %50 ppmA level requiring assessment of the form of boron binding and the specific species

The conversion is simple: 1% by mass = 10,000 ppm by mass . For engineering practice, as important as the total concentration is the information about what portion of boron remains in a state enabling it to effectively interact with the austenite grain boundaries.

Boron and nitrogen, titanium, aluminum and molybdenum – the most important interactions

Boron in steel does not function independently. In metallurgical practice, control of nitrogen (N) is particularly important . Boron readily forms boron nitride (BN). When a significant portion of boron is bound in this form, the hardenability-enhancing effect can be diminished. Therefore, titanium (Ti) is used in many boron steels , which binds nitrogen in stable TiN precipitates.

This approach can limit the formation of BN and increase the amount of effective boron. Aluminum (Al) can also play a role in alloying systems , forming AlN, and molybdenum, the addition of which can limit the unfavorable precipitation of certain borocarbides and alter the optimal boron content. However, neither of these interactions is invariable: the result depends on the composition, temperature, and process.

ElementInteraction with boronTechnological effect
Nitrogen (N)Formation of boron nitride BNPossible limitation of the amount of effective boron
Titanium (Ti)Nitrogen fixation in TiNMay protect boron from binding in BN
Aluminum (Al)Deoxidation and AlN formationIndirect influence on nitrogen balance and release
Molybdenum (Mo)Impact on boron segregation and boron carbide precipitationPossible synergy in increasing hardenability
Carbon (C)It influences the transformations and can co-create boron carbidesIt largely determines the hardness of the resulting martensite

A practical lesson: boron addition should not be assessed solely on the basis of a single line in the chemical composition table. The required properties of steel depend on the entire alloying system and the control of the melting and heat treatment process.

Boron in the microstructure of steel – segregation, nitrides and borides

In steel, boron can occur in several forms. Some atoms remain in solid solution and may segregate at austenite grain boundaries. Another portion binds with nitrogen, forming BN, or participates in the formation of borides and complex precipitates involving other elements. The form of boron presence is as important as its percentage.

Boron dissolved and segregating to grain boundaries

In appropriate amounts, it can delay ferrite nucleation at austenite grain boundaries, increasing hardenability. This effect is particularly pronounced in steels where diffusion transformations limit the possibility of martensite formation at greater depths.

Boron nitride – BN

The formation of BN reduces the pool of boron available to act on grain boundaries. This is one reason why nitrogen control and appropriate nitrogen-binding additives are so important in the production of boron steels.

Borides and borocarbides

An unfavorable combination of boron content, alloy composition, and thermal history can result in the formation of precipitates that do not provide the expected increase in hardenability and, in some materials, impair ductility or fracture toughness. On the other hand, controlled boride precipitates in certain superalloys or boronized layers are deliberately used for other technological purposes.

The influence of boron on the heat treatment of steel

The effectiveness of boron deposition depends on the austenitizing temperature, holding time, and cooling rate. Underheating may not produce the required initial structure, while excessive temperature or insufficient holding time may cause unfavorable segregation changes and the release of boron-containing compounds. Furthermore, excessive temperature promotes austenite grain growth, which may impair selected mechanical properties.

In practice, the required parameters are determined based on the specific grade, component dimensions, delivery condition, and expected hardness and impact strength after machining. Hardenability assessments include CCT charts and Jominy hardenability tests. Boron content alone does not reliably determine hardening temperature or predict hardening depth.

It's also important to remember that increasing hardenability may require adjustments to subsequent tempering. Hardening provides the appropriate structure, while tempering allows for the proper compromise between strength, hardness, ductility, and fracture toughness.

Boron steels – grades and application examples

One of the most well-known applications of boron is in low-alloy manganese-boron steels for hot forming and tool hardening. Boron enables high hardenability without the need for large amounts of costly alloying additives. These materials are particularly important in the automotive industry and in the production of parts requiring high strength.

Example speciesCharacteristicTypical use
22MnB5 / 1.5528Manganese-boron steel with high hardening capacity after austenitizationHot stamping, body safety elements
27MnCrB5Manganese-chromium-boron steel with increased hardenabilitySelected hot-formed and hardened components
37MnB4Manganese-boron steel with a higher carbon content than 22MnB5Structural elements requiring high strength after heat treatment

The list is indicative: the grades differ in standard requirements, composition, intended use, and technological parameters. They are not interchangeable without verifying the documentation and required product properties.

22MnB5 – boron steel for hot stamping

22MnB5 (1.5528) steel is a representative example of the use of boron addition in modern automotive bodywork production. Before the final hardening process, the material can exhibit relatively good formability. During hot stamping, the sheet is heated to the austenitic range, then shaped and rapidly cooled in a specially prepared tool.

Properly performed machining can result in a structure with a high martensite content and a tensile strength of approximately 1500 MPa . This is an approximate value for typical technological solutions, not a guaranteed parameter for every 22MnB5 sheet. The final result depends on the composition, coating, temperature, transfer time, tool pressure, and cooling rate.

This steel is used, among others, in body pillars, sills, reinforcing beams, safety zone elements and structural parts where it is important to reduce weight while maintaining high resistance to deformation.

Boron and the weldability of steel

The presence of boron can indirectly affect weldability by increasing hardenability, thus altering the structure formed in the heat-affected zone. Rapid joint cooling in some boron steels can result in the formation of a hard martensitic microstructure, increasing the risk of cracking under certain conditions. This phenomenon should be analyzed in conjunction with the carbon content, other alloying elements, the amount of diffusible hydrogen, and welding stresses.

The addition of boron does not automatically mean that steel is unweldable. Many boron sheets are industrially joined using spot welding and selected welding methods. However, the appropriate selection of technology is necessary for the grade and condition of the material after forming and hardening. In materials with significant boron content, particularly special neutron-absorbing steels, boride precipitation and localized embrittlement may pose an additional problem.

Boron in stainless steels, heat-resistant steels and special alloys

In conventional stainless steels, boron is not the primary element responsible for corrosion resistance; this role is primarily played by chromium, and in certain environments also by nickel, molybdenum, and nitrogen. However, the addition of boron may have specific technological justifications.

High-temperature and heat-resistant steels

In selected steels with increased chromium content, controlled boron can influence the stability of precipitates and grain boundaries, and thus the material's behavior during long-term operation at elevated temperatures. The interaction with carbides and other precipitate phases is particularly important. The effect depends on the entire alloying system; it cannot be assumed that every boron addition automatically improves creep resistance.

Stainless steels with boron addition – neutron-absorbing materials

A separate group consists of stainless steels with intentionally increased boron content , used, among other things, as thermal neutron absorbers in nuclear power systems. The ¹⁰B isotope is particularly important in this application . Such steels are not equivalent to classic structural steels with a dozen or so ppm of boron – their B content can be many times higher and results from a different material function.

The specialized ASTM A887 standard covers sheet, strip, and plate of chromium-nickel boron-alloyed stainless steels for nuclear applications. These materials require consideration of the effect of borides on formability, processability, and weldability. Selection should consider not only neutron absorption but also mechanical, environmental, and process requirements.

Boron in Nickel Superalloys – Grain Boundaries and Creep Resistance

In many multi-component nickel superalloys, boron serves a different purpose than in typical manganese-boron steels. Very small, controlled additions can segregate into grain boundaries, affecting grain cohesion and the course of intergranular fracture. In a properly designed alloy, this improves creep strength and long-term high-temperature loading.

Borides, including those rich in chromium or molybdenum, which may occur near grain boundaries, are also important in this case. Their effect depends on the amount, size, and distribution. Scattered, controlled precipitates can be beneficial, while excessive amounts or unfavorable boride morphology can impair ductility, complicate processing, and increase the risk of cracking.

Research on various types of superalloys shows that there is no single optimal boron content for all nickel alloys . Results obtained for one alloy, for example, at a specific B level and creep test temperature, cannot be directly transferred to other alloys with different compositions and production technologies. In these materials, boron is a precisely controlled additive, not a universal agent increasing all strength parameters.

Boronizing steel – how is it different from adding boron to molten steel?

Boronizing (boronizing) is a thermochemical treatment process that involves diffusionally saturating the surface layer of a material with boron. It does not involve adding trace amounts of boron to the entire volume of steel during smelting. Its goal is to obtain a surface with high hardness and wear resistance, while retaining a core with properties resulting from the grade used and any prior or subsequent heat treatment.

Depending on the technology, steel boronization is often performed at temperatures in the range of 800–1050°C . Iron boride layers, primarily Fe₂B and Fe₂B , may form on the surface . The Fe₂B layer is sometimes preferred to reduce the risk of cracking that sometimes occurs at the FeB/Fe₂B interface.

  • Fe₂B: approximate microhardness of layers in material tests is approximately 1400–1750 HV, depending on the substrate and process.
  • FeB: can reach around 2000–2300 HV, but higher hardness does not automatically mean better durability of the layer.
  • Advantages: increasing resistance to abrasive and adhesive wear under specific operating conditions.
  • Limitations: risk of brittleness and chipping of the layer in case of unfavorable structure, high impact loads or incorrectly selected thickness.

The hardness of the boride layer in HV units should not be confused with the HRC hardness of the steel throughout its cross-section. These are different measurement cases, with different geometries and microstructures. Boronizing is one of the methods discussed in more detail in the summary of heat and thermochemical treatments of steel.

Boring vs. carburizing, nitriding and hardening – a comparison

The choice of surface hardening technology depends on the type of load, substrate material, operating temperature, required layer depth, and allowable deformation. In particular, boriding should not be automatically replaced with carburizing or nitriding , as the resulting layers have different compositions and hardening mechanisms.

ProcessBasic mechanismTypical goal
DrillingBoron diffusion and boride formationVery hard, wear-resistant layer
Carburizing + hardeningCarbon diffusion, followed by hardening transformationHard layer with a core of selected properties
NitridingNitrogen diffusion and nitride phase formationWear resistance, selected fatigue benefits
Volume hardeningAustenite transformation during coolingChange in structure and properties in cross-section

Advantages of using boron in metallurgy

  • Possibility of significantly increasing the hardenability of selected steels with a very small alloying addition.
  • Better utilization of the cross-section of the hardened element without the need to proportionally increase the content of other additives.
  • Highly suitable for the production of high-strength, hot-formed and hardened automotive parts.
  • Possibility of controlled influence on grain boundaries and creep strength of selected nickel superalloys.
  • Possibility of obtaining exceptionally hard layers in diffusion boriding processes.
  • Special applications of the ¹⁰B isotope in neutron absorbing materials.

Boron-related limitations and risks

  • Nitrogen sensitivity: BN formation may weaken the expected hardenability effect.
  • Narrow range of effective supplement: more boron does not necessarily mean greater hardenability or strength.
  • Sensitivity to heat treatment: austenitizing temperature and cooling process influence boron segregation and precipitation.
  • Risk of fragility: unfavorable borides and other precipitates may impair ductility and fracture toughness.
  • Technological problems: Depending on the material composition and condition, difficulties may occur during welding, forming and heat treatment.
  • There is no simple translation of the content of B into properties: the declaration of the percentage of boron content does not replace the results of material tests.

How to interpret the boron content in the material acceptance certificate?

If steel is to be used in a critical hardened component, it is worth checking not only the grade and boron content provided in the chemical analysis. The requirements of the relevant material standard, other elements, delivery condition, and the conditions of the planned processing are also important.

  • Chemical composition: B content should be verified along with C, Mn, Cr, Mo, N, Ti and Al if relevant for a specific species.
  • Units: you need to distinguish mass percentages from ppm; 0,003% B means 30 ppm, not 0,3%.
  • Material condition: hot stamping sheet, heat-treatable bar and neutron-absorbing steel require a different approach.
  • Required properties: hardness, Rm, yield strength, impact strength and possibly hardenability requirements should be checked – depending on the application.
  • Technology: the final result must be assessed after properly performed heat or thermochemical treatment, and not solely on the basis of the species name.

When purchasing material, it is particularly important to distinguish boron-containing alloy steel from boron-treated steel . The former refers to the chemical composition of the overall alloy; the latter refers to the type of surface treatment.

Frequently asked questions about boron in steel

Does boron increase the hardness of steel?

Primarily, it increases the hardenability of selected steels. The hardness of the finished part can increase if it causes more martensite to form in a given area. However, the maximum martensite hardness strongly depends on the carbon content and the heat treatment condition.

How much boron is enough to improve hardenability?

In many steels, amounts of several to several dozen ppm are sufficient. However, there is no single optimal value for all grades. The amount of boron remaining in an effective form, as well as the nitrogen content and other additives, are important.

Why is titanium used in boron steel?

Titanium binds nitrogen in stable TiN nitrides, which may limit BN formation and allow more boron to interact with the austenite grain boundaries.

Is 22MnB5 steel already hard in the delivered condition?

It doesn't have to be. Its particularly high strength is achieved after properly performed austenitizing, forming, and rapid cooling. The state before and after the process can differ significantly in properties.

Does boron improve the corrosion resistance of stainless steel?

It is not a universal additive for improving the corrosion resistance of stainless steels. In typical steels, chromium plays the main role, and depending on the environment, nickel, molybdenum, and nitrogen also play a role. Boron's importance in special steels often stems from other requirements, such as neutron absorption.

Is boronizing the same as boron steel?

No. Boron steel contains boron in its chemical composition. Boronizing involves diffusionally impregnating the surface with boron to create a hard boride layer.

Summary – The Importance of Boron in Modern Metal Alloys

Boron (B) is one of the most effective micro-alloying additives used to increase the hardenability of selected steels. Its effect is primarily due to its effect on austenite grain boundaries and retarding selected structural transformations during cooling. Achieving this beneficial effect requires control of the effective boron content, nitrogen content, other alloying additives, and heat treatment parameters.

However, the significance of this element is much broader. In nickel alloys, boron can influence the stability of grain boundaries during high-temperature operation, in boronizing processes it enables the production of very hard boride layers, and in special materials with the ¹⁰B isotope, it is used as a neutron absorber. In each of these groups of materials, the purpose of boron addition is different, so properties should always be assessed in relation to the specific alloy and technology.

 

Iron Coal Chromium Nickel Vanadium Manganese Silicon Molybdenum tungsten Copper Tytan Aluminum Cobalt niobium Phosphorus Sulfur Oxygen Nitrogen Magnesium Zinc Bor

Cookie preferences

Dear Customers, the Alfa-Tech website uses cookies to ensure its proper operation. You can specify the conditions for storage or access by clicking Settings . We recommend that you read our Privacy Policy.