10084

 

 

C10E

1.1121

C10R

1.1207

C15E

1.1141

C15R

1.1140

C16E

1.1148

C16R

1.1208

17Cr3

1.7016

17CrS3

1.7014

28Cr4

1.7030

28CrS4

1.7036

16MnCr5

1.7131

16MnCrS5

1.7139

16MnCrB5

1.7160

20MnCr5

1.7147

20MnCrS5

1.7149

18CrMo4

1.7243

18CrMoS4

1.7244

22CrMoS3-5

1.7333

20MoCr3

1.7320

20MoCrS3

1.7319

20MoCr4

1.7321

20MoCrS4

1.7323

16NiCr4

1.5714

16NiCrS4

1.5715

10NiCr5-4

1.5805

18NiCr5-4

1.5810

17CrNi6-6

1.5918

15NiCr13

1.5752

20NiCrMo2-2

1.6523

20NiCrMoS2-2

1.6526

17NiCrMo6-4

1.6566

17NiCrMoS6-4

1.6569

20NiCrMoS6-4

1.6571

18CrNiMo7-6

1.6587

14NiCrMo13-4

1.6657

20NiCrMo13-4

1.6660